切割产生毛刺的处理方法

切割产生的高温会在工件上留下痕迹形成毛刺。材料越热,毛刺就越明显 - 3毫米或更大厚度的毛刺并不少见。其他因素例如钣金件厚度、材料质量及组成,表面以及切割件的温度等也会导致毛刺的形成。此外,设备的加工参数设置也是一个影响因素:人员操作时与最佳切割设置的偏差越大,则切割产生的毛刺就越多。

在等离子切割过程中,如果切割速度过慢,亦会加剧毛刺的形成。综上各种因素作用下,工件的表面就会产生或多或少或大或小的毛刺。与包含许多内切口或内孔的小零件相比,外部轮廓简单的大零件在切割时形成的毛刺会较少些。


相关推荐
新闻聚焦
猜你喜欢
热门推荐
  • Detection of common thread

      Detection of common thread:For the general standard thread, the thread ring gauge or plug gauge is used to measure. In the measurement of external thread, if the thread "over the end" ring is good screw, and the "stop end" ring gauge is not screw into, it indicates that the proce......

    2023-01-01    来源:本站

    分享
  • Fault analysis and handling of electronic expansion valve body

      Fault analysis and treatment of electronic expansion valve body:After confirming that the resistance and joint of the coil part are normal, switch on the power supply of the unit to run, and hold the valve body part by hand to feel whether the valve body is moving. The time from fully open to fully......

    2023-01-01    来源:本站

    分享
  • Analysis and treatment of nozzle failure of electronic expansion valve

      Electronic expansion valve nozzle failure analysis and treatment:1. Apply soapy water to all welding parts and nut connection parts of the pipeline to see if there are bubbles. If there are leaks, reweld or adjust.2. Before the pipeline is rewelded, the valve body should be protected according to th......

    2023-01-01    来源:本站

    分享
  • Failure analysis and treatment of electronic throttle element of electronic expansion valve

      Failure analysis and treatment of electronic throttle element of electronic expansion valve:Open the shell of the electronic throttle element, switch on the power supply of the device, and hold the coil of the electronicexpansion valveby hand to check whether there is any action and whet......

    2023-01-01    来源:本站

    分享
返回列表
Ctrl+D 将本页面保存为书签,全面了解最新资讯,方便快捷。